TY - CONF PB - EDP Sciences AV - none VL - 87 N2 - Ni-Cr based composites with and without the addition of solid lubricants (MoS2, silver and CaF2) were prepared by powder metallurgy method. The samples were sintered at two different temperatures, 1000 °C and 1200 °C. The physical properties such as shrinkage, sintered density and porosity were studied. The microstructures of the Ni-Cr based composites were observed by using SEM analysis while the mechanical properties of the composites were measured by Rockwell Hardness Tester. The results revealed that the increased in sintering temperature improved the shrinkage, sintered density and hardness of the composites while less porosity produced. Ni-Cr based composites with the addition of silver and MoS2 exhibited better shrinkage, density and porosity. Besides, 5 of MoS2 addition in the composites improves the hardness of the composites at sintering temperature 1200°C. © The Authors, published by EDP Sciences, 2017. SN - 2261236X Y1 - 2016/// TI - Physical and Mechanical Properties of Ni-Cr based composites with addition of solid lubricants produced through powder metallurgy process KW - Hardness; Mechanical properties; Metallurgy; Molybdenum compounds; Nickel; Porosity; Powder metallurgy; Shrinkage; Silver; Silver powder metallurgy; Sintering KW - CaF2; MoS2; Physical and mechanical properties; Powder metallurgy process; Rockwell hardness tester; SEM analysis; Sintered density; Sintering temperatures KW - Solid lubricants UR - https://www.scopus.com/inward/record.uri?eid=2-s2.0-85009083852&doi=10.1051%2fmatecconf%2f20178702011&partnerID=40&md5=0a80e3c4363940c7f8cb67534dd66373 N1 - cited By 4; Conference of 9th International Unimas Stem Engineering Conference, ENCON 2016 ; Conference Date: 26 October 2016 Through 28 October 2016; Conference Code:125677 A1 - Mohamad, W.F. A1 - Khan, A.A. A1 - Ahmad, F. A1 - Yassin, A. ID - scholars6537 ER -