eprintid: 1318 rev_number: 2 eprint_status: archive userid: 1 dir: disk0/00/00/13/18 datestamp: 2023-11-09 15:49:28 lastmod: 2023-11-09 15:49:28 status_changed: 2023-11-09 15:39:28 type: article metadata_visibility: show creators_name: Firmanto, H. creators_name: Hussain, P. creators_name: Mamat, O. title: Suppression of iron silicide formation in the reaction layer of sialon-7.5 Cr ferritic steel joint ispublished: pub keywords: Chromium alloys; Diffusion bonding; Diffusion in solids; Ferrite; Silicides, AISI 430 FSS; Iron silicides; Nitrided; Nitrided steels; Reaction layers; Sialon; Silicon diffusion, Ferritic steel note: cited By 0; Conference of 6th International Conference on Diffusion in Solids and Liquids, DSL 2010 ; Conference Date: 5 July 2010 Through 7 July 2010; Conference Code:139479 abstract: Diffusion bonding of sialon and 7.5-Cr Ferritic Steel (FS) in as-received and nitrided condition was studied. Decomposition of sialon and interdiffusion of elements between the sialon and the steel were observed. The interdiffusion of elements produced reaction layers at the joint. The steel moved into the decomposition part of the sialon and replaced the decomposed sialon in this part. Diffusion of silicon into the steel resulted in the silicon-diffusion layer. FeSi2 was formed in the reaction layer when Si in the decomposition part of the sialon reacted with Fe. The use of nitrided steel in the diffusion bonding had suppressed the formation of the FeSi2 in the layer. © (2011) Trans Tech Publications, Switzerland. date: 2010 publisher: Trans Tech Publications Ltd official_url: https://www.scopus.com/inward/record.uri?eid=2-s2.0-84954466863&doi=10.4028%2fwww.scientific.net%2fDDF.312-315.889&partnerID=40&md5=f6c1042eb0ca60b8df287eb959f4cc6c id_number: 10.4028/www.scientific.net/DDF.312-315.889 full_text_status: none publication: Defect and Diffusion Forum volume: 312-31 pagerange: 889-893 refereed: TRUE isbn: 9783037851173 issn: 10120386 citation: Firmanto, H. and Hussain, P. and Mamat, O. (2010) Suppression of iron silicide formation in the reaction layer of sialon-7.5 Cr ferritic steel joint. Defect and Diffusion Forum, 312-31. pp. 889-893. ISSN 10120386